21658 Specimen S1, without a drop panel, could only undergo 2.0% drift (see Figure 8a). After the maximum lateral load of 107 kN was attained, this specimen suddenly failed in brittle punching shear and completely lost its lateral strength and stiffness while no peak load saturation was perceived in advance.